鉛の電解精製におけるにかわの効果の経時変化
https://iwate-u.repo.nii.ac.jp/records/2000492
https://iwate-u.repo.nii.ac.jp/records/20004925da386f6-9493-4837-ae10-48df8572b121
名前 / ファイル | ライセンス | アクション |
---|---|---|
![]() |
|
Item type | 学術雑誌論文 / Journal Article(1) | |||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
公開日 | 2025-01-14 | |||||||||||||
タイトル | ||||||||||||||
タイトル | 鉛の電解精製におけるにかわの効果の経時変化 | |||||||||||||
言語 | ja | |||||||||||||
タイトル | ||||||||||||||
タイトル | Degradation of Glue in Lead Electrorefining | |||||||||||||
言語 | en | |||||||||||||
言語 | ||||||||||||||
言語 | jpn | |||||||||||||
キーワード | ||||||||||||||
言語 | ja | |||||||||||||
主題Scheme | Other | |||||||||||||
主題 | ベッツ法 | |||||||||||||
キーワード | ||||||||||||||
言語 | ja | |||||||||||||
主題Scheme | Other | |||||||||||||
主題 | 電析形態 | |||||||||||||
キーワード | ||||||||||||||
言語 | ja | |||||||||||||
主題Scheme | Other | |||||||||||||
主題 | 高分子添加剤 | |||||||||||||
キーワード | ||||||||||||||
言語 | ja | |||||||||||||
主題Scheme | Other | |||||||||||||
主題 | 過電圧 | |||||||||||||
キーワード | ||||||||||||||
言語 | ja | |||||||||||||
主題Scheme | Other | |||||||||||||
主題 | 分子量 | |||||||||||||
キーワード | ||||||||||||||
言語 | en | |||||||||||||
主題Scheme | Other | |||||||||||||
主題 | Betts Electrolytic Process | |||||||||||||
キーワード | ||||||||||||||
言語 | en | |||||||||||||
主題Scheme | Other | |||||||||||||
主題 | Surface Morphology | |||||||||||||
キーワード | ||||||||||||||
言語 | en | |||||||||||||
主題Scheme | Other | |||||||||||||
主題 | Polymer Additives | |||||||||||||
キーワード | ||||||||||||||
言語 | en | |||||||||||||
主題Scheme | Other | |||||||||||||
主題 | Overpotential | |||||||||||||
キーワード | ||||||||||||||
言語 | en | |||||||||||||
主題Scheme | Other | |||||||||||||
主題 | Molecular Weight | |||||||||||||
資源タイプ | ||||||||||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_6501 | |||||||||||||
資源タイプ | journal article | |||||||||||||
アクセス権 | ||||||||||||||
アクセス権 | open access | |||||||||||||
アクセス権URI | http://purl.org/coar/access_right/c_abf2 | |||||||||||||
著者 |
奥寺, 俊暉
× 奥寺, 俊暉
× 関本, 英弘
|
|||||||||||||
登録日 | ||||||||||||||
日付 | 2025-01-14 | |||||||||||||
日付タイプ | Created | |||||||||||||
書誌情報 |
en : Journal of MMIJ 巻 139, 号 1, p. 1-9, ページ数 9, 発行日 2023-01-31 |
|||||||||||||
ISSN | ||||||||||||||
収録物識別子タイプ | EISSN | |||||||||||||
収録物識別子 | 1884-0450 | |||||||||||||
ISSN | ||||||||||||||
収録物識別子タイプ | PISSN | |||||||||||||
収録物識別子 | 1881-6118 | |||||||||||||
抄録 | ||||||||||||||
内容記述タイプ | Abstract | |||||||||||||
内容記述 | Surface morphology of lead deposits from H2SiF6-PbSiF6 electrolyte containing an animal glue was investigated by means of the periodic galvanostatic electrolysis and SEM-EDS observation. The weight average molecular weight of the glue was also determined with the static light scattering measurement. The temporal changes of the overpotential and the weight average molecular weight were discussed in terms of the elapsed time after preparing the electrolyte which contained 100 g∙L−1 of H2SiF6 and 100 g∙L−1 of Pb(II) and in which the initial concentration of the glue (Cglue) was 0–10.0 g∙L−1. The dendritic growth of lead deposits was observed from the electrolyte of Cglue = 0 g∙L−1 in the galvanostatic electrolysis where the cathodic current density and the electrolyte temperature was −150 A∙m−2 and 40 ℃, respectively. Smooth and dense lead deposits were obtained in the electrolyte of Cglue = 0.5–5.0 g∙L−1 when the elapsed time τ = 0 d. The surface of the deposits gradually became rough with increasing τ in the electrolyte of Cglue = 0.1–1.0 g∙L−1. On the other hand, nodules or bearded deposits were observed on the deposits obtained in the electrolyte of Cglue = 5.0 g∙L−1 when τ = 1–2 d. After this, the surface became smooth with the further increase of τ. The change of the weight average molecular weight of the glue (Mr,w) with τ was described with the equation, 1/(Mr,w)τ = 1/(Mr,w)0 + k′τ, in the electrolyte containing 100 g∙L−1 of free H2SiF6 and 100 g∙L−1 of Pb(II) at 40 ℃. The k′ value was evaluated to be 5 × 10−9 min−1 in the electrolyte of Cglue = 1.0 g∙L−1 and 6 × 10−9 min−1 in the electrolyte of Cglue = 10.0 g∙L−1. | |||||||||||||
言語 | en | |||||||||||||
出版者 | ||||||||||||||
出版者 | 資源・素材学会 | |||||||||||||
言語 | ja | |||||||||||||
出版者 | ||||||||||||||
出版者 | The Mining and Materials Processing Institute of Japan | |||||||||||||
言語 | en | |||||||||||||
権利 | ||||||||||||||
言語 | en | |||||||||||||
権利情報Resource | https://creativecommons.org/licenses/by-nc-nd/4.0/deed.ja | |||||||||||||
権利情報 | Creative Commons Attribution 4.0 International | |||||||||||||
NCID | ||||||||||||||
収録物識別子タイプ | NCID | |||||||||||||
収録物識別子 | AA12188381 | |||||||||||||
DOI | ||||||||||||||
関連タイプ | isIdenticalTo | |||||||||||||
識別子タイプ | DOI | |||||||||||||
関連識別子 | https://doi.org/10.2473/journalofmmij.139.1 | |||||||||||||
著者版フラグ | ||||||||||||||
出版タイプ | VoR | |||||||||||||
出版タイプResource | http://purl.org/coar/version/c_970fb48d4fbd8a85 |